Galvanizing A193 B7 Bolts

The concern with galvanizing any high strength steel is the risk of hydrogen embrittlement. There is plenty of research on galvanizing high strength steels, but conclusions vary on the strength at which hydrogen embrittlement will likely occur when the parts are galvanized. Some research identifies 150 ksi tensile strength as a threshold, but other research indicates that the strength threshold is slightly higher. The documentation that the Bolt Council (Research Council for Structural Connections) cites provides a strength threshold of 39 HRC which equates roughly to 177 ksi.

“The susceptibility of steel fasteners increases significantly when the specified hardness is above 39 HRC (380 HV). Steel fasteners with a specified hardness below 39 HRC (380 HV), normally have no significant susceptibility to hydrogen embrittlement failure.”

Now let’s look at the mechanical requirements of A193 Grade B7, and for comparison purposes, I have included A354 Grade BC.

Grade Marking Specification Material and Treatment Nominal Size (In.) Mechanical Properties Hardness Rockwell
Proof Load Min (ksi) Yield Strength Min (ksi) Tensile Strength Min (ksi) Elong % Min [9] RA % Min [10] Min Max
ASTM A193 Grade B7 A193 Grade B7 Medium Carbon Alloy Steel, Q & T 14" - 212" - 105 125 16 50 - C35
258" - 4" 95 115 16 50 C35
418" - 7" 75 100 18 50 C35
ASTM A354 Grade BC A354 Grade BC 14" - 212" 105 109 125 16 50 C26 C36
258" - 4" 95 99 115 16 45 C22 C33

A193 Grade B7, depending on diameter, has a minimum tensile strength ranging from 100 ksi to 125 ksi. As you stated, there is no maximum strength requirement. So, theoretically, you could have an individual lot of bolts that could exceed 150 ksi or even 177 ksi and therefore raise concern about galvanizing these parts due to hydrogen embrittlement risks. However, there is a maximum hardness requirement ranging from HRC 33 – HRC 36 depending on diameter. Although there is no maximum tensile requirement, the maximum hardness requirement limits the tensile strengths, depending on diameter, to roughly 152 ksi, 160 ksi, or 165 ksi.

Rockwell Rockwell Superficial Brinell Vickers Shore Approx Tensile Strength (psi)
A B C D E F 15-N 30-N 45-N 30-T 3000 kg 500 kg 136 Sciero-scope
60kg Brake 100kg 1/16" Ball 150kg Brake 100kg Brake 100kg 1/8" Ball 60kg 1/16" Ball 15kg Brake 30kg Brake 45kg Brake 30kg 1/16" Ball 10mm Ball Steel Diamond Pyramid
 68.4  109  36  52.3  -  -  78.3  55.9  38.4  -  336  -  354  49  165,000
 67.9  109  35  51.5  -  -  77.7  55.0  37.2  -  327  -  345  48  160,000
 67.4  108  34  5038  -  -  77.2  54.2  36.1  -  319  -  336  47  156,000
 66.8  108  33  50.0  -  -  76.6  53.3  34.9  -  311  -  327  46  152,000

The vast majority of A193 Grade B7 bolts we manufacture falls well below 150 ksi tensile strength due to the limiting factor of the Rockwell hardness requirement. It is rare that a single lot of bolts even approaches 150 ksi tensile strength.

Now let’s take a look at A354 Grade BC as it compares to A193 Grade B7. These two bolt specifications are virtually identical. The difference is their application. A193 bolts are designed for high temperature / high pressure applications, while A354 bolts are used for general purpose applications. They have very similar strength and chemical requirements. As a matter of fact, we make them the exact same way using the exact same raw material and heat-treating procedures. Whereas the ASTM A193 specification makes no reference to galvanizing whatsoever, the A354 Grade BC specification references the option to hot-dip galvanize this grade according to ASTM F2329. In other words, ASTM has no problem with galvanizing a bolt that has a 125 ksi minimum tensile strength requirement with no maximum, and a 36 HRC maximum hardness similar to A193 Grade B7. If ASTM frowned upon galvanizing A193 Grade B7 bolts, they would make a statement within the specification denouncing this practice as they do in other high-strength specifications. Therefore, our position is that A193 Grade B7 bolts can be galvanized with no risk of hydrogen embrittlement.

12 thoughts on “Galvanizing A193 B7 Bolts”

  1. Do you have the material compatibility of SA-193B7 & 194 2H with chemicals or acid services? is it compatible with Chlorate content environments/ plants? should it be galvanized?

Leave a Reply

Your email address will not be published. Required fields are marked *